Metric Coarse Domed Hexagon Nut Low Crown Brass DIN917
Loading...
Zoom

Metric Coarse Domed Hexagon Nut Low Crown Brass DIN917

SKU: 1089
Details
Details
Metric Coarse Domed Hexagon Nut Low Crown Brass DIN917
Dhset
M35.00005.50006.08003.4000
M45.50007.00007.66004.6400
M57.00008.00008.79005.4400
M69.000010.000011.05007.2900
M812.000013.000014.38009.7900
M1014.000017.000018.900011.3500
M1216.000019.000021.100013.8500
M1418.000022.000024.490015.3500
M1620.000024.000026.750017.3500
M1822.000027.000030.140019.4200
M2025.000030.000033.530021.4200
M2228.000032.000035.720022.4200
M2430.000036.000039.980024.4200
M2732.000041.000045.630026.4200
M3034.000046.000051.280028.4200
M3644.000055.000061.310036.5000
M4252.000065.000072.410042.5000
M4858.000075.000083.550048.5000
M5668.000085.000094.690056.6000
M6475.000095.0000105.830062.6000
M7285.0000105.0000116.970067.6000