DA maxA min C square R max F max  F min D
1/4"        0.445        0.435                     0.631/32"       0.186       0.1661/4"
5/16"        0.525        0.515                     0.741/32"       0.228       0.2085/16"
3/8"        0.600        0.585                     0.851/32"       0.270       0.2503/8"
7/16"        0.710        0.695                     1.001/32"       0.312       0.2927/16"
1/2"        0.820        0.800                     1.161/32"       0.363       0.3331/2"
9/16"        0.920        0.900                     1.303/64"       0.405       0.3759/16"
5/8"        1.010        0.985                     1.433/64"       0.447       0.4175/8"
3/4"        1.200        1.175                     1.703/64"       0.530       0.5003/4"
7/8"        1.300        1.270                     1.841/16"       0.623       0.5837/8"
1"        1.480        1.450                     2.091/16"       0.706       0.6661"
1 1/8"        1.670        1.640                     2.361/8"         0.79         0.751 1/8"
1 1/4"        1.860        1.815                     2.631/8"         0.89         0.831 1/4"
1 3/8"        2.050        2.005                     2.901/8"         0.98         0.921 3/8"
1 1/2"        2.220        2.175                     3.141/8"         1.06         1.001 1/2"
1 5/8"        2.410        2.365                     3.411/8"         1.18         1.081 5/8"
1 3/4"        2.580        2.520                     3.651/8"         1.27         1.171 3/4"
2"        2.760        2.700                     3.901/8"         1.43         1.332"
2 1/4"        3.150        3.090                     4.453/16"         1.60         1.502 1/4"
2 1/2"        3.550        3.490                     5.023/16"         1.77         1.672 1/2"
2 3/4"        3.890        3.830                     5.503/16"         1.93         1.832 3/4"
3"        4.180        4.080                     5.913/16"         2.15         2.003"
3 1/4"        4.530        4.430                     6.411/4"         2.32         2.173 1/4"
3 1/2"        4.850        4.750                     6.861/4"         2.48         2.333 1/2"
3 3/4"        5.180        5.080                     7.331/4"         2.65         2.503 3/4"
4"        5.550        5.450                     7.851/4"         2.82         2.674"
4 1/2"        6.380        6.255                     9.021/4"         3.20         3.004 1/2"
5"        7.300        7.175                  10.321/4"         3.53         3.335"
5 1/2"        8.350        8.225                  11.811/4"         3.87         3.675 1/2"
6"        9.450        9.325                  13.361/4"         4.20         4.006"

British standard BS 916

Additional Info
Additional Info
Weight0.0000
MaterialNo
Standard NumberBS1083
Second Standard-
DriveHexagon
HeadSquare
American Generic Brand TermCAP
Diameter 1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.3/4",2.
Length1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5.",5.1/4",5.1/2",5.3/4",6.",6.1/2",7.",7.1/2",8
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.