Metric Coarse 12 Point Flange Head Bolt Stainless-Steel-A2 DIN65438
Loading...
Zoom

Metric Coarse 12 Point Flange Head Bolt Stainless-Steel-A2 DIN65438

SKU: 118
Details
Details
Metric Coarse 12 Point Flange Head Bolt Stainless-Steel-A2 DIN65438
Dds f7dc maxdk minh minkb
M55.00009.10007.77001.00006.50009.0000
M66.000010.60008.91001.20007.500010.0000
M88.000013.600011.18001.60008.600011.5000
M1010.000016.700013.42002.000010.100014.5000
M1212.000019.900015.65002.200011.400016.0000