Metric Coarse Reduced Shank Bolt DIN 931 Grade-8.8 DIN7964D
SKU:
22
Details
Details
Metric Coarse Reduced Shank Bolt DIN 931 Grade-8.8 DIN7964D
d | s | k | b1 | shank max | shank min |
---|
M4 | 7.0000 | 2.8000 | 6.0000 | 3.0000 | 2.8200 |
M5 | 8.0000 | 3.5000 | 8.0000 | 3.5000 | 3.3200 |
M6 | 10.0000 | 4.0000 | 10.0000 | 4.5000 | 4.3200 |
M8 | 13.0000 | 5.3000 | 12.0000 | 5.5000 | 5.3200 |
M10 | 17.0000 | 6.4000 | 15.0000 | 7.0000 | 6.7800 |
M12 | 19.0000 | 7.5000 | 18.0000 | 9.0000 | 8.7800 |
M14 | 22.0000 | 8.8000 | 20.0000 | 11.0000 | 10.7300 |
M16 | 24.0000 | 10.0000 | 24.0000 | 12.0000 | 11.7300 |
Additional Info
Additional InfoWeight | 0.0000 |
---|
Material | Grade-8.8 |
---|
Standard Number | DIN7964D |
---|
Second Standard | - |
---|
Drive | Hexagon |
---|
Head | HEXAGON |
---|
American Generic Brand Term | WAISTED |
---|
Diameter | M4,M5,M6,M8,M10,M12,M14,M16 |
---|
Length | 6,8,10,12,14,16,20,25,30,35,40,45 |
---|