Metric Coarse Structural Hexagon Bolt 1.1/2D HSFG Grade-12.9 DIN6914
Loading...
Zoom

Metric Coarse Structural Hexagon Bolt 1.1/2D HSFG Grade-12.9 DIN6914

SKU: 16
Details
Details
Metric Coarse Structural Hexagon Bolt 1.1/2D HSFG Grade-12.9 DIN6914
Dsekb
M1222.000023.91008.000021.0000
M1627.000029.560010.000026.0000
M2032.000035.030013.000031.0000
M2236.000039.550014.000032.0000
M2441.000045.200015.000034.0000
M2746.000050.850017.000037.0000
M3050.000055.370019.000040.0000
M3660.000066.440023.000048.0000