UNC Link Eye Bolt Forged with Shoulder Collar Steel BS4278T5
d1 B C D E F G H J K L M d Bd Ld
3/4”1.53540.94490.35430.59060.47240.78741.06300.03940.15750.55120.47240.51180.94492.0866
1”1.85041.14170.43310.70870.55120.90551.25980.03940.19690.62990.55120.59061.14172.4803
1.1/4”2.36221.45670.55120.90550.70871.18111.61420.07870.23620.82680.70870.74801.45673.1496
1.1/2”2.95281.81100.66931.14170.90551.49612.04720.07870.27561.02360.90550.94491.81104.0157
1.13/4”3.70082.28350.86611.41731.14171.85042.55910.11810.35431.25981.14171.18112.28354.9606