Metric Coarse Eye Bolt Forged No Shoulder Stainless-Steel-A4 DIN444B

SKU: 138
Details
Details

Metric Coarse Eye Bolt Forged No Shoulder Stainless-Steel-A4 DIN444B

ds Maxs Minb <125b >126 <200b >200d2d3 Maxd3 Min
M565.8816  51211.57
M676.8518  61413.60
M898.852228 81817.57
M101211.822632 102019.48
M121413.82303649122524.48
M161716.82384457163231.38
M202221.79465265184039.38
M242524.80545073224544.40
M272726.7960667924/255049.38
M303029.8066728527/285554.30
M333433.75 7891306059.26
M363837.75 849732/336564.26
M394140.75 9010335/367069.26

 

Metric Coarse Eye Bolt Forged No Shoulder Stainless Steel ss A4 DIN 444 B

Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A4
Standard NumberDIN444B
Second Standard-
DriveNon
HeadEYE
American Generic Brand TermROD END
Diameter M5,M6,M8,M10,M12,M16,M20,M24,M27,M30
Length30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160,170,180,190,200