Metric Coarse Eye Bolt Forged No Shoulder Low grade 4.6 Steel DIN444B
Loading...
Zoom

Metric Coarse Eye Bolt Forged No Shoulder Low grade 4.6 Steel DIN444B

SKU: 135
Details
Details

Metric Coarse Eye Bolt Forged No Shoulder Low grade 4.6 Steel DIN444B

 

ds Maxs Minb <125b >126 <200b >200d2d3 Maxd3 Min
M565.8816  51211.57
M676.8518  61413.60
M898.852228 81817.57
M101211.822632 102019.48
M121413.82303649122524.48
M161716.82384457163231.38
M202221.79465265184039.38
M242524.80545073224544.40
M272726.7960667924/255049.38
M303029.8066728527/285554.30
M333433.75 7891306059.26
M363837.75 849732/336564.26
M394140.75 9010335/367069.26

 

 

Metric Coarse Eye Bolt Forged No Shoulder Low grade 4.6 Steel DIN 444 B