Metric Coarse Eye Bolt Forged No Shoulder Grade-4.6 DIN444A

SKU: 131
Details
Details

Metric Coarse Eye Bolt Forged No Shoulder Grade-4.6 DIN444A

 

ds Maxs Minb <125b >126 <200b >200d2d3 Maxd3 Min
M587.5216  51210.90
M698.5218  61412.90
M81110.302228 81816.90
M101413.302632 102018.70
M121716.30303649122523.70
M161918.16384457163230.40
M202423.16465265184038.40
M242827.20545073224543.40
M273029.1660667924/255048.40
M303433.0066728527/285553.10
M333837.00 7891306058.10
M364140.00 849732/336563.10
M394645.00 9010335/367068.10

 

Metric Coarse Eye Bolt Forged No Shoulder Grade 4.6 DIN 444 A

 

Additional Info
Additional Info
Weight0.0000
MaterialGrade-4.6
Standard NumberDIN444A
Second Standard-
DriveNon
HeadEYE
American Generic Brand TermROD END
Diameter M5,M6,M8,M10,M12,M16,M20,M24,M27,M30
Length30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160,170,180,190,200