BSF Slotted Raised Countersunk Machine Screw Grade-4.8 BS450
d | d | dk max | dk min | k max | f nom | n max | n min | t nom |
---|---|---|---|---|---|---|---|---|
1/8” | 0.1250 | 0.2190 | 0.2010 | 0.0560 | 0.0260 | 0.0390 | 0.0320 | 0.0470 |
3/16” | 0.1875 | 0.3280 | 0.3070 | 0.0840 | 0.0400 | 0.0500 | 0.0420 | 0.0710 |
7/32” | 0.2188 | 0.3830 | 0.3600 | 0.0980 | 0.0440 | 0.0550 | 0.0460 | 0.0830 |
1/4” | 0.2500 | 0.4380 | 0.4120 | 0.1130 | 0.0510 | 0.0610 | 0.0510 | 0.0950 |
5/16” | 0.3125 | 0.5470 | 0.5180 | 0.1410 | 0.0680 | 0.0710 | 0.0610 | 0.1200 |
3/8” | 0.3750 | 0.6560 | 0.6240 | 0.1690 | 0.0800 | 0.0820 | 0.0720 | 0.1440 |