BSW Whitworth Cup Square Neck Carriage Bolt with Nut Grade-4.6 BS325
Loading...
Zoom

BSW Whitworth Cup Square Neck Carriage Bolt with Nut Grade-4.6 BS325

SKU: 2396
Details
Details

BSW Whitworth Cup Square Neck Carriage Bolt with Nut Grade-4.6 BS325

DDF nomF maxF minG maxG minH maxH min
dABCER
1/4"                      0.562                      0.1251/32"0.1881/32"
5/16"                      0.703                      0.1561/32"0.2341/32"
3/8"                      0.844                      0.1881/32"0.2811/32"
7/16"                      0.984                      0.2501/32"0.3281/32"
1/2"                      1.125                      0.2811/32"0.3751/32"
5/8"                      1.406                      0.3751/16"0.4693/64"
3/4"                      1.688                      0.4381/16"0.5623/64"
7/8"                      1.969                      0.5003/32"0.6561/16"
1"                      2.250                      0.5623/32"0.751/16"

 

BSW Whitworth Cup Square Neck Carriage Bolt with Nut Grade-4.6 BS 325 TABLE1