Metric Parallel Dowel Pin Stainless-Steel-A1 DIN7
| dm6 | c | r |
|---|---|---|
| 1.5 | 0.2300 | 1.6000 |
| 2 | 0.3000 | 2.0000 |
| 2.5 | 0.4000 | 2.5000 |
| 3 | 0.4500 | 3.0000 |
| 4 | 0.6000 | 4.0000 |
| 5 | 0.7500 | 5.0000 |
| 6 | 0.9000 | 6.0000 |
| 8 | 1.2000 | 8.0000 |
| 10 | 1.5000 | 10.0000 |
| 12 | 1.8000 | 12.0000 |
| 14 | 2.0000 | 16.0000 |
| 16 | 2.5000 | 16.0000 |
| 20 | 3.0000 | 20.0000 |
| Weight | 0.0000 |
|---|---|
| Material | Stainless-Steel-A1 |
| Standard Number | DIN7 |
| Second Standard | ISO2338 |
| Drive | Non |
| Head | NON |
| American Generic Brand Term | - |
| Diameter | 1.5,2,2.5,3,4,5,6,8,10,12,14,16,20 |
| Length | 2,3,4,5,6,8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160,170,180,190,200 |