Metric Load Indicating Washer DTI with Pips Hardened Steel HSFG BS EN 14399-9
Metric Load Indicating Washer DTI with Pips Hardened Steel BS EN 14399-9
| d | M16 | M20 | M22 | M24 | M27 | M30 | M36 |
| d1 max | 16.85 | 21.05 | 23.15 | 25.25 | 28.40 | 31.55 | 37.85 |
| d2 max | 36.80 | 46.00 | 50.60 | 55.20 | 62.10 | 69.00 | 83.10 |
| d3 max | 25.00 | 29.00 | 33.00 | 38.00 | 43.00 | 46.50 | 56.00 |
| h1 min | 3.00 | 3.50 | 4.00 | 4.00 | 4.00 | 4.00 | 4.00 |
| h2 max | 6.00 | 6.50 | 7.00 | 7.00 | 7.00 | 7.00 | 7.50 |
Metric Load Indicating Washer direct Tension Indicator DTI with Pips Hardened Steel HSFG BS EN 14399-9
| Weight | 0.0000 |
|---|---|
| Material | HARDENED STEEL |
| Standard Number | . |
| Second Standard | - |
| Drive | Non |
| Head | NON |
| American Generic Brand Term | - |
| Diameter | 0 |
| Length | NON |