C50L ROUND HEAD STEEL
| Dia Nom | Grip Min | Grip Max | D Max | E Max | F Nom | PART No | PART No |
|---|---|---|---|---|---|---|---|
| 22.2 | 12.7 | 19.1 | 123.9 | 49.6 | 11.1 | C50LR | BR28-8 |
| 22.2 | 19.1 | 25.4 | 130.2 | 56.0 | 17.5 | C50LR | BR28-12 |
| 22.2 | 25.4 | 31.8 | 136.6 | 62.3 | 23.8 | C50LR | BR28-16 |
| 22.2 | 31.8 | 38.1 | 142.9 | 68.7 | 30.2 | C50LR | BR28-20 |
| 22.2 | 38.1 | 44.5 | 149.3 | 75.0 | 36.5 | C50LR | BR28-24 |
| 22.2 | 44.5 | 50.8 | 155.6 | 81.4 | 42.9 | C50LR | BR28-28 |
| 22.2 | 50.8 | 57.2 | 162.0 | 87.7 | 49.2 | C50LR | BR28-32 |
| 22.2 | 57.2 | 63.5 | 168.3 | 94.1 | 55.6 | C50LR | BR28-36 |
| 22.2 | 63.5 | 69.9 | 174.7 | 100.4 | 61.9 | C50LR | BR28-40 |
| 22.2 | 69.9 | 76.2 | 181.0 | 106.8 | 68.3 | C50LR | BR28-44 |
| 22.2 | 76.2 | 82.6 | 187.4 | 113.1 | 74.6 | C50LR | BR28-48 |
| 22.2 | 82.6 | 88.9 | 193.7 | 119.5 | 81.0 | C50LR | BR28-52 |
| 22.2 | 88.9 | 95.3 | 200.1 | 125.8 | 87.3 | C50LR | BR28-56 |
| 22.2 | 95.3 | 101.6 | 206.4 | 132.2 | 93.7 | C50LR | BR28-60 |
| 22.2 | 101.6 | 108.0 | 212.8 | 138.5 | 100.0 | C50LR | BR28-64 |
| 22.2 | 108.0 | 114.3 | 219.1 | 144.9 | 106.4 | C50LR | BR28-68 |
| 22.2 | 114.3 | 120.7 | 225.5 | 151.2 | 112.7 | C50LR | BR28-72 |
| 22.2 | 120.7 | 127.0 | 231.8 | 157.6 | 119.1 | C50LR | BR28-76 |
| 22.2 | 127.0 | 133.4 | 238.2 | 163.9 | 125.4 | C50LR | BR28-80 |
| 22.2 | 133.4 | 139.7 | 244.5 | 170.3 | 131.8 | C50LR | BR28-84 |
| 22.2 | 139.7 | 146.1 | 250.9 | 176.6 | 138.1 | C50LR | BR28-88 |
| 22.2 | 146.1 | 152.4 | 257.2 | 183.0 | 144.5 | C50LR | BR28-92 |
| 25.4 | 12.7 | 19.1 | 141.6 | 53.9 | 11.1 | C50LR | BR32-8 |
| 25.4 | 19.1 | 25.4 | 148.0 | 60.3 | 17.5 | C50LR | BR32-12 |
| 25.4 | 25.4 | 31.8 | 154.3 | 66.6 | 23.8 | C50LR | BR32-16 |
| 25.4 | 31.8 | 38.1 | 160.7 | 73.0 | 30.2 | C50LR | BR32-20 |
| 25.4 | 38.1 | 44.5 | 167.0 | 79.3 | 36.5 | C50LR | BR32-24 |
| 25.4 | 44.5 | 50.8 | 173.4 | 85.7 | 42.9 | C50LR | BR32-28 |
| 25.4 | 50.8 | 57.2 | 179.7 | 92.0 | 49.2 | C50LR | BR32-32 |
| 25.4 | 57.2 | 63.5 | 186.1 | 98.4 | 55.6 | C50LR | BR32-36 |
| 25.4 | 63.5 | 69.9 | 192.4 | 104.7 | 61.9 | C50LR | BR32-40 |
| 25.4 | 69.9 | 76.2 | 198.8 | 111.1 | 68.3 | C50LR | BR32-44 |
| 25.4 | 76.2 | 82.6 | 205.1 | 117.4 | 74.6 | C50LR | BR32-48 |
| 25.4 | 82.6 | 88.9 | 211.5 | 123.8 | 81.0 | C50LR | BR32-52 |
| 25.4 | 88.9 | 95.3 | 217.8 | 130.1 | 87.3 | C50LR | BR32-56 |
| 25.4 | 95.3 | 101.6 | 224.2 | 136.5 | 93.7 | C50LR | BR32-60 |
| 25.4 | 101.6 | 108.0 | 230.5 | 142.8 | 100.0 | C50LR | BR32-64 |
| 25.4 | 108.0 | 114.3 | 236.9 | 149.2 | 106.4 | C50LR | BR32-68 |
| 25.4 | 114.3 | 120.7 | 243.2 | 155.5 | 112.7 | C50LR | BR32-72 |
| 25.4 | 120.7 | 127.0 | 249.6 | 161.9 | 119.1 | C50LR | BR32-76 |
| 25.4 | 127.0 | 133.4 | 255.9 | 168.2 | 125.4 | C50LR | BR32-80 |
| 25.4 | 133.4 | 139.7 | 262.3 | 174.6 | 131.8 | C50LR | BR32-84 |
| 25.4 | 139.7 | 146.1 | 268.6 | 180.9 | 138.1 | C50LR | BR32-88 |
| 25.4 | 146.1 | 152.4 | 275.0 | 187.3 | 144.5 | C50LR | BR32-92 |
| 28.6 | 41.3 | 54.0 | 178.1 | 90.2 | 40.8 | C50LR | BR36-28 |
| 28.6 | 47.6 | 60.3 | 184.5 | 96.5 | 47.2 | C50LR | BR36-32 |
| 28.6 | 54.0 | 66.7 | 190.8 | 102.9 | 53.5 | C50LR | BR36-36 |
| 28.6 | 60.3 | 73.0 | 197.2 | 109.2 | 59.9 | C50LR | BR36-40 |
| 28.6 | 66.7 | 79.4 | 203.5 | 115.6 | 66.2 | C50LR | BR36 -44 |
| 28.6 | 73.0 | 85.7 | 209.9 | 121.9 | 72.6 | C50LR | BR36-48 |
| 28.6 | 79.4 | 92.1 | 216.2 | 128.3 | 78.9 | C50LR | BR36-52 |
| 28.6 | 85.7 | 98.4 | 222.6 | 134.6 | 85.3 | C50LR | BR36-56 |
| 28.6 | 92.1 | 104.8 | 228.9 | 141.0 | 91.6 | C50LR | BR36-60 |
| 28.6 | 98.4 | 111.1 | 235.3 | 147.3 | 98.0 | C50LR | BR36-64 |
| 28.6 | 104.8 | 117.5 | 241.6 | 153.7 | 104.3 | C50LR | BR36-68 |
| 28.6 | 111.1 | 123.8 | 248.0 | 160.0 | 110.7 | C50LR | BR36-72 |
| 28.6 | 117.5 | 130.2 | 254.3 | 166.4 | 117.0 | C50LR | BR36-76 |
| 28.6 | 123.8 | 136.5 | 260.7 | 172.7 | 123.4 | C50LR | BR36-80 |
| 28.6 | 130.2 | 142.9 | 267.0 | 179.1 | 129.7 | C50LR | BR36-84 |
| 28.6 | 136.5 | 149.2 | 273.4 | 185.4 | 136.1 | C50LR | BR36-88 |
| 28.6 | 142.9 | 155.6 | 279.7 | 191.8 | 142.4 | C50LR | BR36-92 |